Gloss problem in wood finishing.
In finishing world, the term of gloss or sheen is meant by the measurement of lustrous, shininess or
reflecting ability of a surface. The gloss is scaled from 0 sheen to 90 sheen. The
highest gloss or the full gloss is the 90 sheen when the surface reflect all (most of) the
light that come to its surface. While the lower gloss is the 0 sheen, when the
surface absorb all of the light received. Basically the high gloss is resulted by
a flat, even and smooth surface, while the uneven and rough surface will give
the low gloss. See our previous article; gloss in the wood finishing.
Gloss is an important element in the
modern finishing. The gloss will determine the finishing look; the finishing with
same color will give different impression if it has different gloss. The finishing
appearance at the furniture product always needs appropriate gloss instead or finishing color. For example
the carved furniture, the ornamental furniture or the antique furniture usually
need the low or medium gloss finish. While the high gloss is more proper to the
minimalist and the simple furniture.
Now the gloss at the wood finishing
can easily be managed by the selection of the top coat. The top coat as the
final layer of finishing is available in any sheen. The finishing people can choose the top coat with the right sheen according to the finishing requirement.
But as a finishing people, sometime
we face some problems about gloss or sheen in the finishing process. The
gloss could be too low, too high or inconsistent in the finishing. Here some
tips to handle the gloss problem in the wood finishing.
1. The gloss is too low.The low gloss is caused by too much matting agent in the film, uneven film layer or too thin film thickness. Here some tips to solve this problem.
- Always does a good agitation to the top coat mixing
- The coating film is too thin
- A good spray technique.
2. The gloss is too highGloss is too high is usually caused by lack of matting agent content in the film layer, or too thick film layer. Her some tips to solve this problem.
- Do a good agitation to the mixture of top coat.
- Be careful when we use retarder.
- Avoid too thick coating film.
Excellent post. I used to be checking constantly this weblog and I am impressed! Extremely helpful information, I maintain such information a lot. I used to be seeking this certain information for a long time. Thank you and best of luck.
ReplyDeleteThanks & Regards,
Antique Furniture
Thanks for your time to visit us.