High Gloss Black Finish
The high gloss black finish could be the most difficult finishing job in the
wood finishing. The high gloss finish is usually suitable for the furniture
products with simple forms with a clean and neat look. This finish doesn’t
tolerate any imperfectness. The existence of the imperfectness on the product
and the finish will obviously seem. Some small dent, dirt, hole, or gap that could be acceptable for the other color finish will become a big problem
for this finish. If we got the job to do the black high gloss finish, then we should
provide the extra time, energy, materials, and energy to get the perfect
result.
The problems according to the high gloss finish.
The black finish should be a simple process, but actually there are many things that need to be considered to get a good result. The finishing process itself is quite simple; we only need to apply 1 type of stain, the black pigmented stain; it could be the black base coat, black primer, or black enamel. But there are some problems that often arise in the finishing work. The problems could be resulted by the imperfect job at the finishing process, such as the orange peel, uneven gloss, dust spray, dirt, etc. The problems could be from the unfinished wood, such as a gap, uneven surface, gap, hole, dent, crack at the wood, etc. Actually, they are the common problems in the wood finishing, but usually they won’t be visible, obviously, as in the black finish. To make the high gloss finish, then we need to work extra carefully to overcome the problems. In a simple word, the high gloss black finish needs highly precise and perfect work.
Another problem that often arises is the scratch problem at the finished layer. The high gloss finish tends to be scratchy because of his black look. A simple wiping with a cloth to clean the dust on the surface could leave scratch marks, which are clearly visible at this finish. Especially when the “soft” coating material is N.C., shellac, or furniture varnish. To avoid this problem, we need the “hard” coating that is usually more difficult in the handling and application to make the high gloss finish. The proper coating for black high gloss usually is the thermosetting coating, such as PU, AC, UV coating, or polyester coating. They can build the strong and hard film that will avoid the strength problem of this finish, but as chemical reaction coatings, they are more difficult in application
 black high gloss finish
Here are the things to be considered
in the high gloss black finish
- The raw wood preparation.
The high gloss finish will clearly show the texture and condition of the wood
surface. All issues and problems about the imperfectness work at the raw wood,
such as dents, gaps, scratches, cutter marks, pinholes, uneven surfaces, etc.,
will be obviously visible at the final finishing look. Therefore, we need a
good preparation started from the raw wood. A good filler application is needed
to fill in the wood grain and pores.  Any
problems in the unfinished wood should be fixed and corrected. Fill all the
dents, holes, and gaps with putty. Make good sanding to clean any marks and get
an even and smooth wood surface. To get the even surface, then we need the good
sanding machine (wide belt sander or stroke sander) to do the unfinished preparation.
The manual sanding by hand or small hand sander risks resulting in an uneven wood surface that will
clearly appear at the final finish. 
The problems caused by the wood dimensional
changes also should be well anticipated.  Make sure that the timber is already dry and
stable. For the panels, then the engineering wood products such as m.d.f. or
particle board are a better choice than solid wood or veneered wood. The good
m.d.f. or particle board has already a flat surface that is a good base for the
black solid color finish. For the complex form that needs the solid wood, then
we need to make the safe construction. Make
sure the design and construction accommodate the problems due to dimensional
changes in wood.
- The finishing material choice.
This black finishing tends to get problems about scratches or small dents due
to the friction during use, storage, or handling. The small scratches of dents will be obviously visible on this finish. To minimize this problem, then we need
to use the “hard” coating material as the top coat. The shellac, nitrocellulose
coating, lacquer, or other 1-component coating is not suitable for this finish.
The P.U., A.C., or polyester coatings are recommended to make the high gloss
black finish. They will provide a strong finish layer to the final finish and
minimize the scratch problem at the final finish. As a catalyzed coating, they also
give the advantage of giving a thick film built that will help to make the black
finish. 
UV coatings can also be used; they are
strong, build a high thickness of film, and are fast-dry. But the roller application
can be used for the final coating since it will leave the roll mark, which is
not allowed for the high gloss finish. The curtain coater or laser roller might
be able to avoid the roll mark. But it will only work for the flat surfaces. 
- The equipment and finishing room.
To be successful in a black finish, we also need good equipment. The air spray
gun is the best choice to do the coating. It will give the perfect atomization that
is needed to make the perfect finish layering. Make sure the spray gun is in good condition. Any problem in the equipment will result to imperfectness
at the finish layer that won’t be tolerated at this finish. 
The clean and dust-free finishing
room is needed to avoid the dirt and dust problem. Especially when we
consider that we have to apply the PU, AC, or polyester coating that needs a
clean finishing room. 
- Rubbing and polishing.
For the flat surface, then we may consider making the high gloss finish with
rubbing and polishing. The rubbing and polishing will help to solve the
minor problems that always arise at the coating application, such as dust spray, some dirt, thin orange peel, etc. The rubbing and polishing can avoid
the recoating process that requires big effort. The rubbing and polishing can be
used to eliminate the roller marks at the U.V. coating finish to make a high gloss
finish at the flat panels.
Have you ever used black lacquer as an undercoat? If so, what would you recommend as a topcoat to protect it?
ReplyDeleteI am currently using black lacquer on a base plate for a trophy (there is a piece of figured walnut on top of it). It won't see as much handling as a piece of furniture but still requires scratch protection.
You can use the lacquer (NC top coat) as final lacquer.
ReplyDeleteIt is the compatible top coat with your undercoat.
Although it may not as strong as PU or AC, but it works okay for most any finish product.
congratulations guys, quality information you have given!!!
ReplyDeleteclick this site