Swirl marks in wood finishing.
Swirl mark is the problems in the wood finishing process. Swirl mark appears as the swirl or spiral on the wood surface. It will appear more clearly when we apply wood stain on the wood surface. The more stain wet wood the more swirl marks will be apparent. Swirl marks also will be very visible when the glaze is used at the finishing system; the glaze will fill and color the swirl and clearly visible at the finishing result.
Swirl mark problem is caused by the improper sanding process by the hand
sander. The palm sander and rotary disc sander if it is not properly used will
caused the swirl mark. Swirl marks won’t be happened when we sand using the big
sanding machine such as: stroke sander or wide belt sander. The swirl mark is mainly
happened when we press the sanding machine too strong to the wood surface in the
sanding operation. It is often happened when we use the blunt sandpaper or too
fine sandpaper to sand the rough and wood surface.
Here are some tips to handle swirl marks problem.
- Make sure the sanding machine is in good condition.
Palm sander works by vibrate the sandpaper, while the disc sander works by rotating
the sandpaper. Both movements are causing friction with the sandpaper with surface
of the wood. To produce a good sanding result, we need the stable movement. The
unstable movement will cause problems in the sanding result. Put the sandpaper at
the pad and run the machine and feel the movement. The sanding machine must be
able to move and run stable and controllable easily. Stop using sanding machine
when we feel the movement is “wild” and unstable. Fix the sanding machine first
and make sure the machine in the good condition when we run the machine.
The second problem that often found is the pad. The pad is used as a place to
attach the sandpaper that is moved by the machine. The pad needs to be thick and “elastic”
enough to reduce the excessive pressure during the sanding process. Check the
pad condition and make sure it is flat and thick (elastic) enough. The thin and uneven pad
tends to produce excessive pressure on the sanding process which is the main
cause of swirl marks.
- The proper sanding technique.
Hand sander machine is small machine but effective and helpful to do sanding
for small stuff or small area. It is portable handy and flexible with good
result. However, this tool will only work well if we use it properly. The key
is never press the machine too strong. Let the sandpaper does his job to sand
and scrape the wood surface. Just make sure we use the right grade of sandpaper
and use the sharp sandpaper. The sandpaper that has been blunt must be replaced
because it does not work well. Do the sanding process patiently, little by little,
and use the sandpaper grade by grade from the coarse to the finer, never skip
the grade sandpaper. If we push the machine too much then we tend to press the
machine to strong and it will create the swirl mark. (See our previous article : pad sanding machine)
- Checks the sanding before start the finishing process.
- Selection the finishing.
Thanks a lot for publishing the new good stuff for us. I’ll really get the great advantage from your good stuff.