Graining for Wood Finishing
Wood graining is a step in the wood finishing to make
artificial grain. Wood graining is done to make the “wood look” in the
finishing. Wood graining can be performed with the glaze application at the
sealer or base coat (see our previous article: wood graining). The graining can also be done with a wood stain on the raw wood. The graining can be performed by a stain with a particular color (usually
dark brown or black) at the wood to mimic the wood grain. This wood graining
process is done to touch up the puttied wood or to enhance the wood with a vague grain. The wood graining is then followed by the next finishing process
to make the desired color.
Wood graining is art handwork. It needs to be done patiently,
carefully, and cautiously. It is an art to paint the wood. The stain should be at the proper strength.
Too thin stain will make the vague grain look like we cannot make the
grain effect. While too strong stain can bring to the “too artificial grain”
that is not naturally looked.
sand the "too thick stain"
Use a small tip brush (artist brush). Dip the tip of the brush into the wood stain; just dip the tip, not the whole brush; let the tip be wet and hold the stain. We can swap the wet brush with a rag to avoid “too wet stain.". Then brush the stain to line as the grain looked. We can follow the existing wood grain to enhance the vague wood grain, or we can make the new grain line. Do the brushing carefully; make sure the stain line is formed continuously and naturally.
The stain line must be maintained to remain continuous, smooth, and naturally looking. We can sand the stain if the stain is too thick. If necessary, we can use thinner to wipe the stain and reduce the stain strength.
Do carefully check for the graining result before going to the
next finishing process. Any correction for the wood grain can be done before the finishing process. Make sure we got the proper graining, then we can start to do the complete finishing process.
the finish result
Wood graining video



The blog is unique that’s providing the nice material. Please post more interesting articles here.
ReplyDeletemore information here