Crackle Finish with Latex Paint (Latex Paint Effect 2)

Crackle finish is special in the wood furniture finishing. Many people like this finish. In the furniture market, there are many models of crackle-finish furniture. Each has his own unique and beautiful look. In the previous post, I shared about crackle finishing using the NC type material (crackle lacquer). You can go to our previous post: The crackle finish by brush and The crackle finish by spray. 
Now in this article, I want to share the crackle finish with water-base paint (latex paint). The lates paint will give different model crackle effects at the finishing. Actually, there are many water-based crackle paints that are available in paint stores that can be used to generate crackle effects. Some people even can make their own crackle paint. But in here the crackle effect is done by the technique application of the latex paint. The crackle effect is created by heating the latex paint while it is still wet. The heat at the latex paint layer makes the drying process happen rapidly. The fast drying makes the imperfect film build, and a crack-finish layer is resulted.
This method will produce a crackle finish, and the effect can be more managed and adjusted. You can choose the crackle effect on the part you want. The crack effect results only at the heated part. When the paint is drying normally, it won't crack and will keep a smooth finish. The crackle effect resulted is usually smaller and less dramatic than the crackle from crackle paint or crackle lacquer. The crackle depends on the speed of the drying, which can be controlled by the temperature of the hot gun, the speed of gun movement, and also the latex paint thickness.

The finishing process to make crackle finish with latex paint.
  • Sealer application.
Sealer application is the first step to give protection to the wood. The sealer is used as a first layer to avoid the too-wet and pervasive latex paint entering the wood. The solvent-base sealer such as NC, AC, or PU sealer can be used. Apply 2 coats of sealer by wet spray to the overall surface. Let it dry and sand the sealer to make a smooth surface. 


 hot gun

  • Application of latex paint.
This is the step to make the crackle effect. Choose latex paint with the desired color and do the process according to the effect desired.
Spray a wet coat of latex paint evenly. Spray 1 layer or 3 layers of latex paint; make sure you built enough paint layers to make a crackle effect.

Turn on the hot gun and adjust the hot air temperature, then move the gun and direct the hot air to the wet latex paint. The hot gun will blow hot air to heat the latex paint. The latex paint that gets blown with hot air will dry quickly. The rapid drying process will have a rackle effect on the dry paint layer. Adjust the temperature of the hot gun, the distance between the gun and the paint, and the speed of the gun stroke.
Navigate to the hot gun
to the part where the crackle we want. The crackle formed depends on the latex paint type, the thickness of the latex paint, and the heating temperature of the hot gun.  Make sure you got the crackle effect you want


crackle effect from latex paint
  • Application of sealer.
After the crackle effect is obtained, you need to apply a sealer coat to protect the crackle effect. Apply sealer 1 coat evenly on the crackle latex paint, let dry, and do scuff sanding on the sealer.
  • Glaze application
If an antique appearance is needed, then a glaze can be applied here. Apply the glaze with a brush, spray, and wipe. Let the glaze fill and color in the crack to give it a more antique look. Give time to let the glaze dry.
 

 glaze make more antique at the crackle
  •   Top coat application
The top coat is the last finishing layer to provide protection to the finishing obtained. Apply a layer or two layers of top coat by spray coat evenly over the entire surface. For this finish, you need the non-yellowing lacquer with a low gloss to medium gloss. 


Safety in the use of a hot gun.

The hot gun should be treated carefully. This equipment will produce hot air when it is operated. The hot gun contains an electric element that could generate fire. The hot air and the fire from the hot gun is high risk of making fire if exposed to the inflammable solvent and finishing material. When you operated this equipment, you have to keep away from the solvent and finishing material. Do the hot gun application outside the finishing room to minimize the risk of fire.

2 comments for "Crackle Finish with Latex Paint (Latex Paint Effect 2)"

  1. these are all good cares for the furniture, take all the above mentioned steps to care this furniture, buy the kids furniture from this online showroom Kids Bedroom Furniture

    ReplyDelete
    Replies
    1. Thanks for visiting our website.

      God Bless You

      Delete