The finishing for carved wood furniture.

The carving is art to add value for the wood product. The carving is used to give character to the furniture products. The carvings form a special model and look that make the furniture product have more value than just a household product. The carving is a tool to give an artistic touch to the wood product. In the past, the carving could be the only element to build the luxury in the furniture product. Now, there are more tools to build the wood art value, such as inlay, veneer pattern, painting, finishing techniques, etc. But however, the art of woodcarving is still an important tool to add value to the wood furniture. Carving can give the picture or special ornament that gives the soul of the product.



the carved wood furniture with a natural finish

Finishing for carved product.

To maximize the added value, the carved furniture requires a proper finishing. The finishing on carved wood should be done with the proper technique. Some points that need to be considered:
  • The stain application.
Carving is a process of cutting the wood; the carving part is a piece of wood with an end grain. This part will tend to absorb more stain than the surface wood. Too wet stain application can lead to the absorption of too much color, resulting in too dark color on the carving part. Application staining by brush or wipe should be carefully done. The application by brush should be done with the thin stain; the thick stain is risky to get too dark.
The spray application is a better choice because, by this method, your stain will be controlled better. Do medium wet spray technique for staining, and since the carved is rather complicated, it may be rather difficult to get the even coloration with 1 layer of spray. You better dilute the stain and spray stain in two layers instead of spraying 1 layer with thick stain.
  • Sealer application.
The carved part is end grain that will absorb more coating. It needs more clear coating layers to make a smooth surface. You need to put an extra layer on the carved part when applying the sealer and top coat. Some people do sealer application and sand the wood carved before stain application. This method will make the carving more subtle and reduce the risk of absorbing too much stain on the staining.
  • Sanding.
The carving sections have uneven surfaces; he needs a special sanding tool that can follow the shape and pattern of the carving. A rigid sandpaper will tend to cut the tip of the carving and deform the engraving pattern. It needs flexible abrasives. The sanding of the unfinished wood should be done with cloth sandpaper. The cloth-backed sandpaper is flexible to follow the carved form and has less risk of deforming the carved shape. While sanding the sealer or top coat, you better use Scotch-Brite. Scotch brite is quite flexible and be able to follow the carving shapes and reach the inside part. 



glaze effect in the wood-carved furniture

The applicaton of glaze.

Glaze is the perfect finishing material to enhance and highlight the carved wood. Glaze with the right application will produce the beautiful, alive appearance by enhancing the carved form. Glaze will also be able to fill and color the inside carving part easily and overcome the difficulties in the staining.
Brush the glaze on the carving and let it fill the inside of the carving and all crevices evenly, and then do highlights (wipe a little bit of glaze on the outside part). The highlighted glaze will produce a finishing with more vivid coloration and enhance the form and shape of the carving.
The glaze should be applied on the sealer when the carved part is smooth and has enough film built. The carving part with a thin clear coating is usually rough and risky to absorb too much glaze and result in a too-dark color.
If the glaze is applied over the wash coat, then it should be preceded by the application of an inert (glaze base) first. Brush or spray the inert glaze to wet the carving part, then apply the glaze thereon, then brush the glaze evenly. The inert will fill the end grain to avoid the glaze penetrating too much and preventing too much coloration. 

2 comments for "The finishing for carved wood furniture."

  1. sealer sending and glaze is very much important when need to finish the furniture, here is the one such great resource for the online furniture shoppers, buy Kids Bedroom Furniture there are very much added feature when need to buy from the online furniture showroom.

    ReplyDelete
    Replies
    1. Yes. agree.

      Thanks you for visit our website

      GBU

      Delete