Hardness Test for the Wood Finishing
The finishing industry needs some standard quality for their
product. The big furniture company that sells big-volume products usually sets a quality
standard for his product. There are some tests held to ensure
his products fulfill the standard quality that has been set up. When he goes to his vendor, he always does some testing to make sure his product fulfills the quality. When he sells his product, then he can show the test result to convince and attract his buyer.
One of the
common tests for the wood finishing layer is the hardness test. The hardness
test is a test to determine the hardness of the finish layer. There are several methods that can be
held for testing the
hardness. Now in this article we want to share about the pencil test to do the hardness test. This
method covers a
procedure for rapid,
inexpensive, and easy to determine the film hardness
of a given coating.
The complete test method is according to the ASTM
D3359 standard.
The tool required
- A set of drawing graphite leads pencils that meet the following scale of hardness.
These pencils come in various degrees
of hardness, following the 6B-5B-4B-3B-2B-B-(HB-F)-H-2H-3H-4H-5H-6H, and are generally supplied by any
leading pencil manufacturer. The grade of a pencil is determined by the amount
of baked graphite and clay in its composition.
- Sandpaper
- A piece of wood finish panel as a subject for testing.
- Apparatus for the test
the apparatus to do the hardness test
How the test is held.
Sand the tip
or the lead with #400 grade sandpaper to make his tip absolutely flat with a sharp circumcenter edge.
the pencil tip is sanded to get flat with a sharp circumcenter edge.
Place the
finish panel on a level, firm, horizontal surface. The pencil is held firm in the testing
tool. Then move the test tool 3 inches forward on the film surface in the direction of wood grain at an angle of 45 degrees. Started with the pencil
hardness HB-F, then repeat this process up
the hardness scale until a pencil is found that cuts through to the substrate
for a distance of at least 3 mm. The hardness scale is based on the pencil where
the finish is uncut. For example, if the finish fails at HB-F, then the hardest of
the finish is "the B graphite pencil.". If the defect is already found with the HB-F, then the result is the softer pencil.
the pencil is moved on the finish




The finishing industry needs some standard quality for their product. The big furniture company that sell big volume product usually set a quality standard for his product. dynapocket hardness tester
ReplyDeleteYes it is. The woodworking tool has also provide many equipments and tools to do the standard test.
ReplyDeleteThanks You for visiting and commenting i here.
commenting
ReplyDelete