Oil Problem in Pine Wood
Pine wood is one of the most popular in the wood industry. Pine trees are much planted to green the mountain, and the
wood is used for industrial purposes. The pulp,
chemicals, or woodworking are the industries that use the
pine timber. In the woodworking industry, pine wood is used to make many wood products. It is used as material for making furniture, house frames, doors, windows, and flooring parquet. The pine wood has many species; about 125 species are known. The character
of the pine wood may vary depending on the species and the place it grows. But generally it is soft wood, with a light yellow base
color, and inexpensive. The wood has a strong character of grain but with fewer pores and grain texture, which makes the wood liked by the wood furniture manufacturer. With the
proper finishing, it can produce a wood product with a beautiful and attractive appearance.
But the pine wood needs to be handled properly. The wood has oil that could lead to problems if it is not well handled. The pine oil is actually resin that is useful in the chemical industry, but it may interfere with the utilization of the wood in the woodworking. The pine oil may interfere with the color of the finished wood. In the waxed finish, the oil from pine wood could make the wax difficult to dry. The oil will mix with the wax and stay as a sticky wax. For wood finishes with thick pigment, such as the solid color finish or wash finish, the oil will come out as a yellow stain that will ruin the finishing look. Since that, the oil in pine wood should be anticipated to make good products in the woodworking industry.
But the pine wood needs to be handled properly. The wood has oil that could lead to problems if it is not well handled. The pine oil is actually resin that is useful in the chemical industry, but it may interfere with the utilization of the wood in the woodworking. The pine oil may interfere with the color of the finished wood. In the waxed finish, the oil from pine wood could make the wax difficult to dry. The oil will mix with the wax and stay as a sticky wax. For wood finishes with thick pigment, such as the solid color finish or wash finish, the oil will come out as a yellow stain that will ruin the finishing look. Since that, the oil in pine wood should be anticipated to make good products in the woodworking industry.
 the oil in the pine wood
How to overcome the oil problem from the pine wood.
The oil comes out together with the release of water vapor from the wood. The wet wood has a higher risk of getting the oil problem. For a wide and big surface, then the use of wood veneer is a better option. Veneer is cheaper and can be easier selected before it is laminated to the core. Veneer is also a thin layer, which has less oil than the thick, solid wood. Veneer is also marketed in dry conditions, making it less risky for the oil problem.
- Choose the proper finishing.
 the pine oil bleeds in the white finish
- Selection and treatment of the wood.
The oil comes out together with the release of water vapor from the wood. The wet wood has a higher risk of getting the oil problem. For a wide and big surface, then the use of wood veneer is a better option. Veneer is cheaper and can be easier selected before it is laminated to the core. Veneer is also a thin layer, which has less oil than the thick, solid wood. Veneer is also marketed in dry conditions, making it less risky for the oil problem.
- Use the oil block.
The oil block will affect the stain absortbion that will affect the color. Since that, it should be used only for solid color or wash finish. You don't need the oil block for the transparent finish color. The oil block even can ruin the transparent finish since it will interfere with the stain absorption by the wood.
Apply
the oil block sealer by brush or spray at the wood knot, and let it dry. It usually needs
about a few minutes to dry, then sand the sealer before starting the finishing process.

Thanks for sharing. Despite the fact that pine home furniture tend to be much less popular these days you are able to find lots of suppliers. A number of them can be found online where they offer amazing deals.
ReplyDeleteThanks for visit us.
DeleteYes pine wood is less popular now. There are still many furniture are made from pine wood.
Good luck
Pine trees could be the most abundant tree species in the world. I do believe that using and patronizing pine wood furniture is environmentally sustainable because it does not threaten the extinction of this species. Some companies manufacturing it label themselves as "Carbon Neutral" because they support and maintain tree plantations that help absorb ozone-depleting gases. :)
ReplyDeleteThis comment has been removed by the author.
DeleteSolid pine is high on demand because it could be used in a wide variety of furniture styles. I live how it could be shaped in variety of forms and engraved intricately due to its fine and soft grain.
ReplyDeleteyes it is. Pine wood offer many advantages. it is "cheap" with abundant resources. It is also quite easy to be handled and processed in the woodworking.
DeleteThanks
Good luck