The Trembesi Wood for Furniture
The trembesi tree (Albizia saman) is much cultivated throughout the tropical area. It grows best in the lowlands from sea level to 500 m (1640 ft) with rainfall of 600–3000 mm (24–120 in). The tree can grow fast and become big timber in the proper climate. It usually reaches 15–25 m height with a wide canopy leaf and big-diameter log. In Indonesia, the tree is planted in large quantities at the road as a shade tree for reforestation. The saman tree is chosen to green the land since it is fast-growing and a good absorber for CO₂ from the air. In Indonesia, the action of planting the trembesi tree is encouraged in many areas. The wood is available in Indonesia by many names, such as tamarind, munggur, ki hujan, trembesi, meh, etc.
trembesi wood panel
Since its availability, some furniture manufacturers have used the trembesi wood to
make furniture. It is quite cheap and easy to be handled in the
woodworking industry. It can be used to make indoor furniture in combination
with veneer or other wood species. The wood has strong grain character with
shallow pores and grain texture; with the proper finishing, it can produce an
attractive appearance. This wood has a medium hardness, making it relatively easily machined, drilled, or sanded in the woodworking process. Some furniture manufacturers also use this wood for outdoor furniture, with a quite good result.
But the wood
is always unique; each type of wood has a special character that is different from
the other. The trembesi as a product from trees also has special characteristics that
need to be well anticipated to get them maximum benefit.
trembesi solid wood furniture
There are some things that need to be considered in the process of tamarind wood.
- The insect attacked.
The tamarind
wood has a risk of getting attacked by insects. Although the risk of insect attack is not as high as with the mahogany or mango wood, it is still recommended to do chemical treatment to prevent the insect problem. The chemical treatment at the planks before they dried in the kiln dry oven. or at the dry-sawn timber will minimize the insect problem in the future.
- The volume shrinkage.
The trembesi wood
has high volume shrinkage from the wet to the dry wood. It has a high risk for
rupture and bending. Therefore, he must be dried properly; the drying process
cannot be too fast since the risk of damaged and broken wood. After the wood is
dry, it needs to be layered with the proper finishing layer to minimize the
risk of wood movement. The finishing layer will coat the wood, make it stable, and minimize the wood movement.
trembesi finish panel
- The finishing for trembesi.
The trembesi
wood contains some oils inside. The oil is not as much as teak wood oil, but it
could interfere with the finished look. To minimize the oil problem, we need to dry the wood at the standard m.c. and choose the proper
finishing color. The antique brown transparent finishing color is the best
choice for this wood. The wood has nice grain patterns that can be maximized
with the transparent color. It has the white color base at the sapwood and
brown to dark brown at the heartwood. Finishing with dark brown color
is the easiest to achieve. If the light color finish is needed, then we may
need to bleach the dark wood.
The finishing
with solid color can also be generated, but we must be aware of the oil
inside the wood. We need to apply the oil block (insulator) at the first step to prevent
the oil from coming true and ruining the finish.



I have a table made from a trunk of this rainwood , I've noticed it seems to be getting g darker , could this be from the oil coming to the surface?
ReplyDeleteI've noticed the same over time
ReplyDeleteyes it might be.
DeleteYoung girls in indonesia are so sympathics .
ReplyDelete