Aluminum antique finish
Aluminum as a
furniture substrate may be much less than the wood, but the aluminum furniture
is quite well popular in the market. Aluminum is much used to make metal furniture
since it is easily handled, machined and shaped and have high durability. Aluminum
in various model and shape can be found in many furniture products. (See our
previous article: aluminum for furniture). Although aluminum can be exposed in
the unfinished state, but we can finish the aluminum to produce more attractive
appearance and more durable product. There are many finishing models and color can
be generated for the aluminum, and now in this article we want to share the
antique finish for aluminum. It it’s the finishing for aluminum with the application of stain
and glaze with special techniques same as finishing process in the wood
furniture finishing.
- 1. Application of metal primer coat.
In this finish basically we used the finishing process with NC finishing
material. To generated good adhesion to the finishing layer then a the metal primer coat is needed. It is the paint or coating that
serves to do as the "connector" between the NC finish with the metal. It is applied as the first coating on the metal before the application of NC or varnish, stain or
glaze application. In this finishing process we used a clear metal primer (no
color metal primer), since we want to make a semi transparent finish. The primer
metal coat was layered as the first coat by spray wet evenly the aluminum surface.
Then we waited for about 30 minutes to let the coat dry.
- 2. Application of stain.
Stain was used to color the aluminum to produce the desired finish color. We
used a black toner stain. Toner stain is a stain with some clear coat in the
mixture. We mixed black stain with some vinyl sealer (about 5 %) to make the
toner. The sealer in the stain mixed helps the stain to attach better for the
aluminum surface. The black toner was sprayed evenly all over the aluminum
surface. The toner stain color blended with the basic color of the aluminum metal to make
a dark aluminum metal color. To make antique effect and more life impression, we did
some highlight to the stain. We wiped slightly the stain layer with steel
wool at some parts to make more life finishing looked.
- 3. Application of clear coating.
The next process is the sealer application. One coat of vinyl sealer was
layered on the stain to provide protection layer to the stain and give smooth surface
before glaze application. Vinyl sealer was applied by spray evenly all over the surface. We let the vinyl sealer layer for about 20 minutes to dry.
application glaze to make antique
- 4. Application of glaze.
Glaze was applied to form the dark black color and to make antic effect in the finishing.
Glaze was poured to overall surface and wiped off by rag and brushed to get the even layer of glaze coat.
Some highlighted with the steel wool was
done to produce the antique and old looked impression. We let the glaze for about
60 minutes to dry.
- 5. Application of top coat.
After the glaze layer is dry, then we blown the glaze layer to clean it for the
steel wool dust or any other dirt. We also checked the color and effect of the
finish, to make sure we got the proper color and effect before we applied the top
coat layer. We sprayed 15 sheen NC top coat as the last layer. We waited for 30
minutes until the top coat layer to dry, and we checked the film layer and finished
color resulted. Since we got rough surface, then we did lightly scuff sanding
to the top coat and applied one more layer of top coat. The result was an
antique black metal aluminum finish.
I am really appreciating very much by seeing your interesting posts.
ReplyDeleteclick here for more info