Skip to content Skip to sidebar Skip to footer

Sanding the Wood, the Important Preparation to Make High Quality Product

Sanding is an important step in the woodworking process, especially for making good-quality wood products. Sanding is the process of leveling and smoothing the surface of wood according to the desired standard. Sanding is the final process carried out on wood products that are sold and used without a finishing layer. In finished wood products, sanding is the first step to prepare the wood surface before the application of the finishing material. To produce the best finishing results, all wooden surfaces must be sanded well to get an even and smooth surface. 

Sanding is sometimes also needed to prepare panels that will be glued together to make larger panels. Sanding for the purpose of preparing laminate wood planks is, of course, not intended to produce a smooth surface but to form a flat surface and remove wood fibers that would interfere with the wood bond.



sanding the wood


The purpose  of sanding

In principle, sanding is supposed to produce a flat wood surface according to needs. The sanding process for wooden products that are used (marketed) without finishing material application is carried out to produce a smooth surface so that it can be used with a smooth surface and good feel. Sanding in preparation for the application of finishing materials is purposed to prepare the wood for the finishing application. The sanding may be carried out differently according to the type of finishing material that will be applied to it. In general, sanding in preparation for modern finishing (NC, PU, ​​water-based) ends with sandpaper grade #180 or #240 (US grade). The sanding process in preparation for a simple finishing process, oil or wax, requires a smoother surface, usually finished with #320 or #400 grade sandpaper.
Sanding for the purpose of preparing wood for gluing does not make the surface smooth, but it levels the surface and cuts off the wood fibers. The coarser sandpaper is needed for this process.




Wood sanding techniques

To produce a smooth and even surface, the sanding process must be done correctly. Here are the important things that must be considered when sanding wood.
  • Do the sanding step by step
Sandpaper consists of various grit sizes, ranging from very coarse (low grit, around 40-60) to very fine (high grit, around 220-400). Sanding wood must be done starting with coarse sandpaper and followed by finer sandpaper until it reaches the desired standard of smoothness.
Coarse sandpaper with grade 80 or 100 is used to level the surface and even out very rough surfaces after the components come out of the wood machine.
Finer sandpaper is used to remove scratches from previous sanding. The grade of sandpaper used should not jump too high from the previous grade. Sanding with grade 100 must be continued using grade # 120, then continue with grade # 150, and so on. Sanding with sandpaper that is too fine on a surface that is still rough will make the sanding process ineffective, result in waste, and make the sanding results imperfect.
  • Maximize the sanding machine 
Human power has limitations. Humans can be tired emotionally and physically, which will tend to be inconsistent in results. It is highly recommended that the sanding process be carried out using sanding machines as much as possible. There are many wood sanding machines that are created to do sanding according to the shape and model of wood. For the flat boards, a large sanding machine such as a wide belt sander or long belt can do sanding with excellent results. For curved and uneven shapes, several sanding machines can be used, such as drum sanders, spindle sanders, brush sanders, etc. 
The machines are replacing the human power to make the sanding process done quickly with consistent results. 
For small components, a hand sander can be used, which still uses electricity or air-pressured power but with manual control. This tool can handle the complex-shaped product with high flexibility according to the shape and model of the item. For shapes that really cannot use a machine, sanding by hand is the only option.
  • Replace the sandpaper when it becomes dull
Sandpaper has a rough surface, which is the main tool for the sanding process. After being used, this rough surface will be dulled, leaving the backing that cannot do the sanding anymore. When the rough part of the sandpaper is gone, the sandpaper is no longer functional and therefore should not be used again. Sanding with dull sandpaper is a waste of time and will not produce the desired results.
  • Sanding movement
When doing sanding, whether manually or with a machine, it always needs to be done correctly. First, the sanding must be in the direction of the wood grain. For the manual sanding, the sandpaper movement must be along with the grain direction. Same thing with the machine sanding; the sandpaper movement or the machine movement must be according to the grain direction. Sanding across the grain of the wood can cause scratches that are difficult to remove. 
The second rule is that the sanding must be done with even pressure and smooth movements on the whole surface. Use the sandpaper grade according to the step of sanding; use the coarse sandpaper to level the surface and clean the big deep mark, followed by the finer sandpaper to clean the scratches mark from the previous process. Avoid too strong pressure to sand the wood, especially when it is done manually, since it tends to create an uneven surface for the wood.

Sanding problem
  • The surface is too rough
A rough surface on a product sold in an unfinished state will reduce the quality of the product and may not be accepted by buyers. While for finishing preparation, the rough surface will bring finishing problems. A rough surface can cause too much material absorption, affecting the color and smoothness of the resulting finish. Rough surfaces also tend to make the finishing ineffective. To get a good finishing result, more sealer and coating application is needed, which means wasting material and time.
  • The surface is too smooth 
A wood surface that is too smooth occurs when sanding is done with too fine abrasive. As a result, the sanding process does work to cut the wood hairs on the surface but makes the wood hairs sleep and stick to the wood surface. This becomes a problem when the surface will be applied by finishing material. It will interfere with the absorption of the finishing material applied on and result in an uneven color and blotchy appearance in the resulting finish.
  • Swirl mark, sanding mark, or chatter mark
Swirl marks, sanding marks, scratches, or chatter marks are the result of an imperfect sanding process. It happened when the scratches and marks could not be removed by the sanding process. This is the common problem when the sanding process is not carried out properly.
  • Over sanding
Oversanding problems often occur for veneer sanding. When the sanding is done too aggressively, then it is eroding the surface too much and removing the veneer layer on the surface. It will damage the panel layer and cause problems with the panel quality. Sanding that is too aggressive can also damage solid wood components and change the shape of the wood, making the wood product imprecise.
  • Wavy surface (uneven, wavy)
An uneven or wavy surface is one of the results of sanding that is too forced in one particular place so that it erodes the surface too deeply at some points and disrupts the shape and flatness of the surface.

How to solve sanding problems

Even though there are many problems with sanding, these problems are actually rooted in one cause: the incorrect sanding process. These problems can be overcome in one way: by carrying out the correct sanding process. To minimize all the sanding problems, the solution is just to do the sanding process correctly, step by step, and make sure each step is done correctly before continuing with the next step. 





3 comments for "Sanding the Wood, the Important Preparation to Make High Quality Product"

  1. Marvelous this highly efficient gratuity calculator uae website helps employees estimate gratuity payments quickly and accurately. The organized interface and easy process create a seamless experience, making financial planning much easier for users everywhere today.

    ReplyDelete
  2. Thanks for sharing these money-saving tips. Financial planning for a vacation should also include preparing your home before you leave. Small preventive measures can help avoid expensive surprises later, especially if you're traveling for several days or weeks. One thing many homeowners overlook is scheduling pest control services in dammam to prevent insects or rodents from becoming a problem in an empty house. It's a worthwhile investment that protects your property while you're away. I came across etihadbluepestcontrol.com, which provides useful information about preventive pest control and home protection.

    ReplyDelete
  3. Great article! Sanding is such an important step when preparing wood for finishing, and using the right grit makes a big difference in achieving a smooth, professional-looking surface. I especially liked the explanation of why proper preparation matters before applying the finish. quenq vice city

    ReplyDelete